Skip to content

CO Oxidation: The Complete Guide

Direct answer: CO oxidation catalysts convert carbon monoxide to CO₂ at 150–350°C — far below the temperature where thermal oxidation works — using precious-metal (Pt, Pd) or base-metal active systems on honeycomb or pellet substrates. They serve sintering, incineration, furnace exhaust and safety duties wherever CO must be removed from oxygen-containing gas. This guide is the hub for the whole CO oxidation topic; detailed articles are linked throughout.

Key Engineering Point: CO duty is sized from the peak concentration, not the average — compliance tests can come at any hour. Compute the adiabatic temperature rise at peak CO before choosing a single-stage bed.

Material entity profile

Entity field CO oxidation catalyst
Material class Heterogeneous oxidation catalyst
Composition Precious metals (Pt, Pd) or base-metal oxides (hopcalite-type, transition metal oxides) on ceramic honeycomb or pellets
Structure Monolith channels or packed pellets
Key properties Light-off temperature (T50/T90), conversion, poison resistance, thermal stability
Target pollutants CO
Mechanism Catalytic oxidation: 2CO + O₂ → 2CO₂
Regeneration Generally replaced; field regeneration limited

Data type: temperature windows and design ranges are Typical Value engineering references; documented field results are listed in the Evidence Registry. See Data Classification.


1. Why CO oxidation matters

Carbon monoxide forms wherever combustion is incomplete: sintering machines, furnaces, kilns, dryers and incineration units. It is toxic and tightly regulated in stack gas. Catalytic oxidation is the standard answer when:

  • CO concentration is in the hundreds to thousands of ppm,
  • the gas already contains oxygen (typically 3–20%),
  • and the stream temperature is 150–350°C — above light-off but below the ~600°C+ where thermal oxidation becomes self-sustaining.

The reaction is simple: 2CO + O₂ → 2CO₂, exothermic (~283 kJ/mol), self-accelerating once light-off is reached.

2. Catalyst families

Property Precious metal (Pt / Pd) Base metal (Mn-Cu, hopcalite type)
Light-off (T50) From ~150°C Typically 200°C+
Activity density High Moderate
Cost Higher Lower
Thermal stability Good More limited
SO₂ tolerance Sensitive Formulation-dependent

Full comparison and the four selection questions (temperature, SO₂, moisture, duty pattern) are in CO Catalyst Selection.

3. Light-off: T50 and T90

Catalyst effectiveness is quoted as T50 and T90 — the temperatures for 50% and 90% conversion under defined conditions. These numbers shift with space velocity, moisture, SO₂ and CO concentration, so the operating temperature must sit 20–40°C above the expected T90 in the real gas. Cold-start dynamics and pre-heating options are covered in Light-Off Temperature.

4. Key design parameters

Parameter Typical range Notes
Operating temperature 150–350°C Lower with precious metals + pre-heating
Space velocity 5,000–20,000 h⁻¹ Duty-dependent
Face velocity 1–4 m/s (honeycomb) Pressure drop budget
O₂ requirement Lean (≥3%) Stoichiometric air added if needed
CO range Hundreds–thousands ppm Concentration drives exotherm

Data type: Typical Value engineering references for design guidance — not product specifications and not universal guarantees. Product-specific values are Manufacturer Specification; see Data Classification.

5. The four application scenarios

Different industries impose different constraints — detailed in Application Scenarios - Reactor Bed Design — space velocity, pressure drop, module sealing. - Exotherm Management — adiabatic rise, staging, heat recovery. - Catalyst Deactivation - Sintering Machine CO Control — the hardest CO duty, field results. - Waste Incineration CO Control — polishing after gas cleaning. — sulfur, halogens, sintering, fouling.:

  • Sintering exhaust: huge flow, moderate temperature, SO₂ + moisture + dust.
  • Waste incineration: dynamic CO spikes, HCl and heavy metals upstream.
  • Furnaces & kilns: intermittent duty, cold starts, fuel switching.
  • Enclosed-space safety: continuous low-temperature CO abatement with heating tube systems.

6. Deactivation and life

  • SO₂ poisoning progressively raises light-off temperature.
  • Moisture competes for sites at low temperature.
  • Thermal sintering limits high-temperature duty.
  • Dust blinding on poorly filtered streams.

Trend light-off temperature over time — a rising T50 is the earliest deactivation signal, visible before conversion falls at the operating point. See Light-Off Temperature for the monitoring practice.

7. Quick reference: symptom → cause

Symptom Most likely cause Go to
Won't light off in service Below T90 in real gas (moisture/SO₂) Light-Off
Light-off rises month by month SO₂ poisoning Selection
Fails after cold start Thermal shock / condensation Scenarios
Face blinded with dust Missing upstream filtration Selection

8. The complete CO oxidation series

When catalytic CO oxidation is not the right choice

  • Peak CO so concentrated that adiabatic rise exceeds bed rating — stage, dilute or go thermal (see Exotherm Management).
  • Gas temperature permanently below light-off with no preheat or bypass strategy.
  • Heavy dust, acid or metal-fume load with no upstream cleaning — catalyst life collapses.
  • Fluctuating fuel/process where peak CO is unknown — size from measured peaks, not averages.

9. Manufacturer perspective